08X22H6T Stainless Steels

08X22H6T - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 08X22H6T grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.80
Mn - 0.80
P - 0.035
S - 0.025
Cr 21.00 23.00
Ni 5.30 6.30
Mo - 0.30
W - 0.20
Ti 5×C 0.65

08X22H6T - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 08X22H6T

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
379 (≥) 643 (≥) 23 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade 08X22H6T

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
889 (≥) 656 (≥) 13 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
154 873 898

Equivalent Grade

Equivalent Products

We can customize the production of 08X22H6T grade, contact us for the best solution.