0Cr18Ni12Mo3Ti Stainless Steels to GB 13296 (2007)

0Cr18Ni12Mo3Ti - Specification & Application

  • GB 13296 (2007) - Seamless stainless steel tubes for boiler and heat exchanger
  • GB 2270 (1980) - Seamless tubes
  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 14975 (2002) - Stainless steel seamless tubes for structures
  • GB/T 14976 (2002) - Stainless steel seamless tubes for fluid transport
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates

Seamless stainless steel tubes for boiler and heat exchanger

Chemical composition(wt.%) of 0Cr18Ni12Mo3Ti grade: to GB 13296 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 11.00 14.00
Cr 16.00 19.00
Mo 2.50 3.50
Ti - 5xC%-0.70

0Cr18Ni12Mo3Ti - Detail

0Cr18Ni12Mo3Ti

Mechanical properties of grade 0Cr18Ni12Mo3Ti GB 13296 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
887 (≥) 781 (≥) 32 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade 0Cr18Ni12Mo3Ti GB 13296 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
284 (≥) 574 (≥) 21 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
985 197 244

Equivalent Grade

Equivalent Products

We can customize the production of 0Cr18Ni12Mo3Ti grade, contact us for the best solution.