1.2361 Tool Die Steels

1.2361 - Specification & Application

High alloyed CrMoV steel

Chemical composition(wt.%) of 1.2361 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.86 0.96
Si - 1.00
Mn - 1.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Mo 0.90 1.30
V 0.07 0.12
Ni - 0.30

1.2361 - Detail

High alloyed CrMoV steel

Mechanical properties of grade 1.2361

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
422 (≥) 419 (≥) 34 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade 1.2361

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
271 (≥) 461 (≥) 43 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
417 528 272

Equivalent Grade

Equivalent Products

We can customize the production of 1.2361 grade, contact us for the best solution.