1.2376 Tool Die Steels to DIN 17350 (1980)

1.2376 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of 1.2376 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.92 1.00
Si 0.20 0.40
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 11.00 12.00
Mo 0.80 1.00
V 0.80 1.00

1.2376 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade 1.2376 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
286 (≥) 369 (≥) 23 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade 1.2376 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
716 (≥) 215 (≥) 34 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
499 481 252