1.3802 Stainless Steels to DIN EN 10349

1.3802 - Specification & Application

  • DIN EN 10349 - Steel castings - Austenitic manganese steel castings
  • SEW 395 - Non magnetizable steel casting. Technical delivery conditions

Steel castings - Austenitic manganese steel castings

Chemical composition(wt.%) of 1.3802 grade: to DIN EN 10349

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.10 1.30
Si - 0.50
Mn 11.50 13.50
P - 0.060
S - 0.030
Cr - 0.50

1.3802 - Detail

Steel castings - Austenitic manganese steel castings, 1-3802 GX120Mn13

Mechanical properties of grade 1.3802 DIN EN 10349

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
777 (≥) 178 (≥) 44 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 1.3802 DIN EN 10349

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
147 (≥) 865 (≥) 12 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
637 884 639