100V1 Tool Die Steels

100V1 - Specification & Application

High carbon steel

Chemical composition(wt.%) of 100V1 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.05
Si 0.15 0.25
Mn 0.15 0.30
P - 0.025
S - 0.025
Cr - -
Mo - -
V 0.10 0.15

100V1 - Detail

High carbon steel

Mechanical properties of grade 100V1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
268 (≥) 989 (≥) 33 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade 100V1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
288 (≥) 283 (≥) 34 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
298 593 858

Equivalent Grade

Equivalent Products

We can customize the production of 100V1 grade, contact us for the best solution.