102CrMo6 Tool Die Steels

102CrMo6 - Specification & Application

Alloyed CrMo steel

Chemical composition(wt.%) of 102CrMo6 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.98 1.05
Si 0.50 0.65
Mn 1.00 1.15
P - 0.020
S - 0.020
Cr 1.40 1.60
Mo 0.12 0.17
V - -

102CrMo6 - Detail

Alloyed CrMo steel

Mechanical properties of grade 102CrMo6

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
759 (≥) 964 (≥) 44 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade 102CrMo6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
269 (≥) 828 (≥) 14 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
385 135 383

Equivalent Grade

Equivalent Products

We can customize the production of 102CrMo6 grade, contact us for the best solution.