10X14AΓl5 Stainless Steels

10X14AΓl5 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 10X14AΓl5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.80
Mn 14.50 16.50
P - 0.045
S - 0.030
Cr 13.00 15.00
Ni - 0.60
Mo - -
W - -
Ti - 0.20
N 0.15 0.25

10X14AΓl5 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 10X14AΓl5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
282 (≥) 944 (≥) 21 44 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade 10X14AΓl5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
263 (≥) 748 (≥) 43 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
217 217 469

Equivalent Grade

Equivalent Products

We can customize the production of 10X14AΓl5 grade, contact us for the best solution.
sales@specificsteel.com