10X15H27T3MP Stainless Steels

10X15H27T3MP - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 10X15H27T3MP grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.60
Mn - 0.60
P - 0.020
S - 0.010
Cr 14.00 16.00
Ni 25.00 28.00
Mo - 0.30
Nb 0.70 1.00

10X15H27T3MP - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 10X15H27T3MP

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
889 (≥) 689 (≥) 44 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade 10X15H27T3MP

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
464 (≥) 233 (≥) 23 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
493 258 211

Equivalent Grade

Equivalent Products

We can customize the production of 10X15H27T3MP grade, contact us for the best solution.