125CrSi5 Tool Die Steels

125CrSi5 - Specification & Application

Alloyed SiCr steel

Chemical composition(wt.%) of 125CrSi5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.20 1.30
Si 1.05 1.25
Mn 0.60 0.80
P - 0.035
S - 0.035
Cr 1.10 1.30
Mo - -
V - -

125CrSi5 - Detail

Alloyed SiCr steel

Mechanical properties of grade 125CrSi5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
871 (≥) 273 (≥) 13 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade 125CrSi5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
964 (≥) 767 (≥) 22 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
476 247 472

Equivalent Grade

Equivalent Products

We can customize the production of 125CrSi5 grade, contact us for the best solution.