142WV13 Tool Die Steels

142WV13 - Specification & Application

Alloyed WV steel

Chemical composition(wt.%) of 142WV13 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.35 1.50
Si 0.15 0.30
Mn 0.20 0.40
P - 0.035
S - 0.035
Cr 0.20 0.50
Mo - -
V 0.20 0.30
W 2.80 3.30

142WV13 - Detail

Alloyed WV steel

Mechanical properties of grade 142WV13

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
694 (≥) 447 (≥) 41 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade 142WV13

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
691 (≥) 421 (≥) 14 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
351 496 278

Equivalent Grade

Equivalent Products

We can customize the production of 142WV13 grade, contact us for the best solution.