15NiCr14 Tool Die Steels

15NiCr14 - Specification & Application

Alloyed NiCr steel

Chemical composition(wt.%) of 15NiCr14 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.17
Si 0.20 0.35
Mn 0.30 0.50
P - 0.030
S - 0.030
Cr 0.65 0.85
Mo - -
V - -
Ni 3.30 3.60

15NiCr14 - Detail

Alloyed NiCr steel

Mechanical properties of grade 15NiCr14

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
836 (≥) 468 (≥) 24 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade 15NiCr14

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
871 (≥) 712 (≥) 44 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
362 725 132

Equivalent Grade

Equivalent Products

We can customize the production of 15NiCr14 grade, contact us for the best solution.
sales@specificsteel.com