Chemical composition(wt.%) of 15X25T grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 0.80
P - 0.035
S - 0.025
Cr 24.00 27.00
Ni - 0.60
Mo - -
W - -
Ti 5×C 0.90

15X25T - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 15X25T

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
161 (≥) 655 (≥) 34 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade 15X25T

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
214 (≥) 283 (≥) 24 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
652 112 116

Equivalent Grade

Equivalent Products

We can customize the production of 15X25T grade, contact us for the best solution.