15X5 Stainless Steels

15X5 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 15X5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.50
Mn - 0.50
P - 0.030
S - 0.025
Cr 4.50 6.00
Ni - 0.60
Mo 4.50 6.00
W - -
Ti - -

15X5 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 15X5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
995 (≥) 827 (≥) 32 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 15X5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
629 (≥) 393 (≥) 11 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
269 919 738

Equivalent Products

We can customize the production of 15X5 grade, contact us for the best solution.