1OXl1H20T2P Stainless Steels

1OXl1H20T2P - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 1OXl1H20T2P grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.020
Cr 10.00 12.50
Ni 18.00 21.00
Mo - 0.30
Ti 2.30 2.80
Al - 0.50

1OXl1H20T2P - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 1OXl1H20T2P

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
493 (≥) 323 (≥) 13 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade 1OXl1H20T2P

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
639 (≥) 559 (≥) 32 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
358 755 781

Equivalent Grade

Equivalent Products

We can customize the production of 1OXl1H20T2P grade, contact us for the best solution.