20X13 Stainless Steels

20X13 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 20X13 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16 0.25
Si - 0.80
Mn - 0.80
P - 0.030
S - 0.025
Cr 12.00 14.00
Ni - 0.60
Mo - -
W 1.60 2.00
Ti - 0.20

20X13 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 20X13

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
717 (≥) 764 (≥) 14 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade 20X13

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
667 (≥) 213 (≥) 23 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
387 265 558

Equivalent Products

We can customize the production of 20X13 grade, contact us for the best solution.