216 Stainless Steels

216 - Specification & Application

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of 216 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.75
Mn 7.50 9.00
P - 0.045
S - 0.03
Cr 17.5 22.0
Ni 5.00 7.00
Mo 2.00 3.00
N 0.25 0.50

216 - Detail

AISI 216

Mechanical properties of grade 216

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
175 (≥) 475 (≥) 42 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade 216

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
674 (≥) 822 (≥) 13 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
574 557 633
We can customize the production of 216 grade, contact us for the best solution.