21MnCr5 Tool Die Steels to DIN 17350 (1980)

21MnCr5 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery
  • DIN EN ISO 4957 (1999) - Tool steels (ISO 4957:1999)

Tool steels (ISO 4957:1999)

Chemical composition(wt.%) of 21MnCr5 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.18 0.24
Si 0.15 0.35
Mn 1.10 1.40
P - 0.030
S - 0.030
Cr 1.00 1.30
Mo - -
V - -

21MnCr5 - Detail

Tool steels (ISO 4957:1999)

Mechanical properties of grade 21MnCr5 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
446 (≥) 951 (≥) 11 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 21MnCr5 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
637 (≥) 611 (≥) 11 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
852 995 843

Equivalent Grade

Equivalent Products

We can customize the production of 21MnCr5 grade, contact us for the best solution.
sales@specificsteel.com