2564 Stainless Steels to SS 142564

2564 - Specification & Application

  • SS 142564 - Stainless steel for castings

Stainless steel for castings

Chemical composition(wt.%) of 2564 grade: to SS 142564

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 19.00 21.00
Ni 24.00 26.00
Mo 4.00 5.00
Cu 3.00 3.50

2564 - Detail

Stainless steel for castings

Mechanical properties of grade 2564 SS 142564

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
678 (≥) 776 (≥) 32 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade 2564 SS 142564

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
591 (≥) 454 (≥) 41 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
267 524 119

Equivalent Products

We can customize the production of 2564 grade, contact us for the best solution.