25X18H10B2 Stainless Steels

25X18H10B2 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 25X18H10B2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.21 0.28
Si 0.30 0.80
Mn - 0.70
P - 0.030
S - 0.030
Cr 17.00 19.00
Ni 9.00 11.00
Mo - 0.30
W 2.00 2.50

25X18H10B2 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 25X18H10B2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
951 (≥) 913 (≥) 14 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade 25X18H10B2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
191 (≥) 846 (≥) 42 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
888 892 658

Equivalent Grade

Equivalent Products

We can customize the production of 25X18H10B2 grade, contact us for the best solution.