27CrMoV5-7 Stainless Steels to NF EN 10269

27CrMoV5-7 - Specification & Application

  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(wt.%) of 27CrMoV5-7 grade: to NF EN 10269

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.25
Si - 0.40
Mn 0.40 0.80
P - 0.030
S - 0.030
Cr 1.20 1.50
Ni - 0.60
Mo 0.55 0.80
V 0.20 0.35
Al 0.030 -

27CrMoV5-7 - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade 27CrMoV5-7 NF EN 10269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
225 (≥) 856 (≥) 12 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade 27CrMoV5-7 NF EN 10269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
351 (≥) 479 (≥) 11 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
875 267 669