303Se Stainless Steels to G3067

303Se - Specification & Application

  • G3067 - Stainless steel bars
  • G3077 - Stainless steel wire rods
  • G3076 - Stainless steel wires

Stainless steel wire rods

Chemical composition(wt.%) of 303Se grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.20
S - 0.06
Ni 8.00 10.00
Cr 17.00 19.00
Mo - -
Se 0.15 -

303Se - Detail

Stainless steel wire rods

Mechanical properties of grade 303Se G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
248 (≥) 942 (≥) 23 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade 303Se G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
688 (≥) 951 (≥) 23 34 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
186 235 239

Equivalent Products

We can customize the production of 303Se grade, contact us for the best solution.
sales@specificsteel.com