309S Stainless Steels to A 213/A 213M (2011)

309S - Specification & Application

  • A 213/A 213M (2011) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
  • A 240/A 240M (2012) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications
  • A 249/A 249M (2010) - Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
  • A 276 (2010) - Stainless Steel Bars and Shapes
  • A 312/A 312M (2012) - Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes
  • A 314 (2008) - Stainless Steel Billets and Bars for Forging
  • A 358/A 358M (2008) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications
  • A 409/A 409M (2009) - Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service
  • A 473 (2009) - Stainless Steel Forgings
  • A 478 (2008) - Chromium-Nickel Stainless Steel Weaving and Knitting Wire
  • A 479/A 479M (2011) - Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
  • A 511/A 511M (2012) - Seamless Stainless Steel Mechanical Tubing
  • A 554 (2011) - Welded Stainless Steel Mechanical Tubing
  • A 580/A 580M (2012) - Stainless Steel Wire
  • A 813/A 813M (2009) - Single- or Double-Welded Austenitic Stainless Steel Pipe
  • A 814/A 814M (2008) - Cold-Worked Welded Austenitic Stainless Steel Pipe
  • A 943/A 943M (2009) - Spray-Formed Seamless Austenitic Stainless Steel Pipes
  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
  • SAE J 405 (1998) - Chemical compositions of SAE wrought stainless steels
  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Chemical compositions of SAE wrought stainless steels

Chemical composition(wt.%) of 309S grade: to A 213/A 213M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 22.0 24.0
Ni 12.0 15.0

309S - Detail

Chemical compositions of SAE wrought stainless steels

Mechanical properties of grade 309S A 213/A 213M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
378 (≥) 831 (≥) 44 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade 309S A 213/A 213M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
936 (≥) 274 (≥) 33 21 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
681 771 684

Equivalent Products

We can customize the production of 309S grade, contact us for the best solution.