329J3L Stainless Steels to G3067

329J3L - Specification & Application

  • G3067 - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of 329J3L grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Ni 4.50 6.50
Cr 21.00 24.00
Mo 2.50 3.50
N 0.08 0.20

329J3L - Detail

Stainless steel bars

Mechanical properties of grade 329J3L G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
519 (≥) 415 (≥) 41 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade 329J3L G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
339 (≥) 179 (≥) 21 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
749 596 657

Equivalent Products

We can customize the production of 329J3L grade, contact us for the best solution.