329J4L Stainless Steels to G3067

329J4L - Specification & Application

  • G3067 - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of 329J4L grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 1.50
P - 0.040
S - 0.030
Ni 5.50 7.50
Cr 24.00 26.00
Mo 2.50 3.50
N 0.08 0.30

329J4L - Detail

Stainless steel bars

Mechanical properties of grade 329J4L G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
817 (≥) 665 (≥) 34 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 329J4L G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
374 (≥) 169 (≥) 44 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
365 863 123

Equivalent Products

We can customize the production of 329J4L grade, contact us for the best solution.