347TKA Stainless Steels

347TKA - Specification & Application

CNS standard mechanical and structure with stainless steel pipe

Chemical composition(wt.%) of 347TKA grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 17.00 19.00
Ni 9.00 13.00
Mo - -
Nb 10×C% -

347TKA - Detail

CNS standard mechanical and structure with stainless steel pipe

Mechanical properties of grade 347TKA

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
674 (≥) 742 (≥) 12 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade 347TKA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
425 (≥) 492 (≥) 41 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
295 855 445

Equivalent Products

We can customize the production of 347TKA grade, contact us for the best solution.