403Cb(ESR) Stainless Steels

403Cb(ESR) - Specification & Application

403Cb(ESR)

Chemical composition(wt.%) of 403Cb(ESR) grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.13 0.18
Si - 0.50
Mn 0.40 0.60
P - 0.025
S - 0.010
Cr 11.00 13.00
Mo - 0.20
Ni - 0.60
Nb 0.15 0.25
V - 0.10
Pb - 0.005
Sn - 0.05
Al - 0.05

403Cb(ESR) - Detail

403Cb

Mechanical properties of grade 403Cb(ESR)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
688 (≥) 994 (≥) 14 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade 403Cb(ESR)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
324 (≥) 684 (≥) 33 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
381 119 466
We can customize the production of 403Cb(ESR) grade, contact us for the best solution.