45X14H1482M Stainless Steels

45X14H1482M - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 45X14H1482M grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si - 0.80
Mn - 0.70
P - 0.035
S - 0.020
Cr 13.00 15.00
Ni 13.00 15.00
Mo 0.25 0.40
W 2.00 2.80
Ti - 0.20

45X14H1482M - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 45X14H1482M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
881 (≥) 697 (≥) 34 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade 45X14H1482M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
831 (≥) 732 (≥) 11 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
336 944 175

Equivalent Grade

Equivalent Products

We can customize the production of 45X14H1482M grade, contact us for the best solution.
sales@specificsteel.com