60MnSiCr4 Tool Die Steels to DIN 17350 (1980)

60MnSiCr4 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of 60MnSiCr4 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.58 0.65
Si 0.80 1.00
Mn 0.80 1.20
P - 0.030
S - 0.030
Cr 0.20 0.40
Mo - -
V - -

60MnSiCr4 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade 60MnSiCr4 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
356 (≥) 553 (≥) 34 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade 60MnSiCr4 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
517 (≥) 849 (≥) 12 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
637 231 499