632J1CPS Stainless Steels

632J1CPS - Specification & Application

CNS standard spring cold rolled stainless steel strip

Chemical composition(wt.%) of 632J1CPS grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si 1.00 2.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 13.50 15.50
Ni 6.50 7.55
Cu 0.40 1.00
Ti 0.20 0.65

632J1CPS - Detail

CNS standard spring cold rolled stainless steel strip

Mechanical properties of grade 632J1CPS

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
396 (≥) 241 (≥) 43 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 632J1CPS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
839 (≥) 745 (≥) 23 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
881 522 118

Equivalent Grade

Equivalent Products

We can customize the production of 632J1CPS grade, contact us for the best solution.
sales@specificsteel.com