70Si7 Tool Die Steels

70Si7 - Specification & Application

Alloyed Si steel

Chemical composition(wt.%) of 70Si7 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.65 0.75
Si 1.50 1.80
Mn 0.60 0.80
P - 0.030
S - 0.030
Cr - -
Mo - -
V - -

70Si7 - Detail

Alloyed Si steel

Mechanical properties of grade 70Si7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
743 (≥) 952 (≥) 12 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade 70Si7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
674 (≥) 237 (≥) 12 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
177 724 618

Equivalent Grade

Equivalent Products

We can customize the production of 70Si7 grade, contact us for the best solution.