95X18 Stainless Steels

95X18 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 95X18 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.90 1.00
Si - 0.80
Mn - 0.80
P - 0.030
S - 0.025
Cr 17.00 19.00
Ni - 0.60
Mo - -
W - 0.20
Ti - 0.20

95X18 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 95X18

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
727 (≥) 244 (≥) 31 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade 95X18

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
999 (≥) 358 (≥) 31 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
346 524 683

Equivalent Grade

Equivalent Products

We can customize the production of 95X18 grade, contact us for the best solution.