A 182 F 316Ti Stainless Steels to A 182/A 182M (2012)

A 182 F 316Ti - Specification & Application

  • A 182/A 182M (2012) - Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Chemical composition(wt.%) of A 182 F 316Ti grade: to A 182/A 182M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N - 0.10
Ti - 5(C+N)≤Ti≤0.70

A 182 F 316Ti - Detail

Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Mechanical properties of grade A 182 F 316Ti A 182/A 182M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
872 (≥) 572 (≥) 32 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade A 182 F 316Ti A 182/A 182M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
484 (≥) 524 (≥) 42 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
134 213 154

Equivalent Products

We can customize the production of A 182 F 316Ti grade, contact us for the best solution.