AISI501 Stainless Steels

AISI501 - Specification & Application

AISI501

Chemical composition(wt.%) of AISI501 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 -
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 4 6
Mo 0.40 0.65

AISI501 - Detail

AISI501

Mechanical properties of grade AISI501

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
734 (≥) 534 (≥) 32 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade AISI501

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
316 (≥) 352 (≥) 41 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
443 224 526

Equivalent Products

We can customize the production of AISI501 grade, contact us for the best solution.