ASTM501 Stainless Steels

ASTM501 - Specification & Application

ASTM501

Chemical composition(wt.%) of ASTM501 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
c 0.10 -
Si - 0.10
Mn - 0.10
P - 0.04
S - 0.03
Cr 4.00 6.00
Mo 0.40 0.65

ASTM501 - Detail

ASTM501

Mechanical properties of grade ASTM501

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
491 (≥) 848 (≥) 23 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade ASTM501

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
673 (≥) 743 (≥) 44 12 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
857 966 672

Equivalent Products

We can customize the production of ASTM501 grade, contact us for the best solution.
sales@specificsteel.com