ASTMXM-25 Stainless Steels

ASTMXM-25 - Specification & Application

ASTMXM-25

Chemical composition(wt.%) of ASTMXM-25 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Si - 1.00
Mn - 1.00
P - 0.03
S - 0.03
Cr 14.0 16.0
Ni 5.00 7.00
Mo 0.50 1.00
Cu 1.25 1.75
Nb 8×C% -

ASTMXM-25 - Detail

ASTMXM-25

Mechanical properties of grade ASTMXM-25

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
432 (≥) 928 (≥) 22 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade ASTMXM-25

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
743 (≥) 686 (≥) 41 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
897 117 282

Equivalent Products

We can customize the production of ASTMXM-25 grade, contact us for the best solution.