CNS 201 Stainless Steels to G3067

CNS 201 - Specification & Application

  • G3067 - Stainless steel bars
  • G3076 - Stainless steel wires
  • G3077 - Stainless steel wire rods

Stainless steel wire rods

Chemical composition(wt.%) of CNS 201 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn 5.50 7.50
P - 0.060
S - 0.030
Ni 3.50 5.50
Cr 16.00 18.00
Mo - -
N - 0.25

CNS 201 - Detail

Stainless steel wire rods

Mechanical properties of grade CNS 201 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
245 (≥) 242 (≥) 33 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade CNS 201 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
822 (≥) 258 (≥) 21 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
924 537 857

Equivalent Products

We can customize the production of CNS 201 grade, contact us for the best solution.