CNS 403 Stainless Steels to G3067

CNS 403 - Specification & Application

  • G3067 - Stainless steel bars
  • G3076 - Stainless steel wires
  • G3077 - Stainless steel wire rods

Stainless steel wire rods

Chemical composition(wt.%) of CNS 403 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.50
Mn - 1.00
P - 0.040
S - 0.030
Ni - 0.60
Cr 11.50 13.00
Mo - -

CNS 403 - Detail

Stainless steel wire rods

Mechanical properties of grade CNS 403 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
533 (≥) 799 (≥) 22 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade CNS 403 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
295 (≥) 818 (≥) 14 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
835 823 849
We can customize the production of CNS 403 grade, contact us for the best solution.
sales@specificsteel.com