CNS 434 Stainless Steels to G3067

CNS 434 - Specification & Application

  • G3067 - Stainless steel bars
  • G3077 - Stainless steel wire rods

Stainless steel wire rods

Chemical composition(wt.%) of CNS 434 grade: to G3067

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Ni - -
Cr 16.00 18.00
Mo 0.75 1.25

CNS 434 - Detail

Stainless steel wire rods

Mechanical properties of grade CNS 434 G3067

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
694 (≥) 464 (≥) 12 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade CNS 434 G3067

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
765 (≥) 546 (≥) 43 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
683 481 139

Equivalent Products

We can customize the production of CNS 434 grade, contact us for the best solution.