CU-5 Special Alloy

Chemical composition%of the ladle analysis of gradeCU-5

C(%)W(%)Co(%)Nb(%)Ta(%)
5.277.016.00.31.5
CU-5
Density / (g/cm ^ 3) : 13.90
Hardness HRC: 87.5
σ bb/MPa: 2710
Grain size/μ m: 1 ~ 2
Use for example: can be used in the manufacture of the impact of medium under the mould

Mechanical properties of gradeCU-5

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
575(≥) 591(≥) 14 33 22 Solution and Aging,Annealing,Ausaging,Q+T,etc 242

Physical properties of grade CU-5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
962(≥) 839(≥) 12 23 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
731 661 917

CU-5 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade