EVl4 Stainless Steels

EVl4 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EVl4 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 -
Si 0.40 -
Mn 6.50 -
P - -
S - -
Cr 21.0 -
Ni 5.50 -
N 0.20 -

EVl4 - Detail

Steel for exhaust valves

Mechanical properties of grade EVl4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
974 (≥) 286 (≥) 44 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade EVl4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
243 (≥) 343 (≥) 22 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
591 332 417

Equivalent Grade

Equivalent Products

We can customize the production of EVl4 grade, contact us for the best solution.