F10004 Cast Iron and Cast Steel to A 159 (2011)

F10004 - Specification & Application

  • A 159 (2011) - Automotive Gray Iron Castings

Used in the products of the automobile, truck, tractor, and allied industries. Miscellaneous soft iron castings (as cast or annealed) in which strength is not of primary consideration. Exhaust manifolds may be made of this grade of iron, alloyed or unallo

Chemical composition(wt.%) of F10004 grade: to A 159 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 3.40 3.70
Si 2.30 2.80
Mn 0.50 0.80
P - 0.25
S - 0.15
CEV 4.25 4.5

F10004 - Detail

F10004

Mechanical properties of grade F10004 A 159 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
849 (≥) 765 (≥) 32 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade F10004 A 159 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
415 (≥) 834 (≥) 11 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
274 136 765

Equivalent Grade

Equivalent Products

We can customize the production of F10004 grade, contact us for the best solution.