Fe-Ni47Cr5 Stainless Steels to NF A 54-301

Fe-Ni47Cr5 - Specification & Application

  • NF A 54-301 - Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Chemical composition(wt.%) of Fe-Ni47Cr5 grade: to NF A 54-301

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - 0.20
Mn - 0.40
P - 0.030
S - 0.030
Cr - 5.00
Ni - 47.00
Mo - -
Fe - remaining(48.00)

Fe-Ni47Cr5 - Detail

Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Mechanical properties of grade Fe-Ni47Cr5 NF A 54-301

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
858 (≥) 352 (≥) 12 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade Fe-Ni47Cr5 NF A 54-301

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
848 (≥) 245 (≥) 21 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
835 195 593