GH3128 Stainless Steels to GB/T 14992 (2005)

GH3128 - Specification & Application

  • GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
  • GB/T 14995 (2010) - Hot-rolled superalloy sheets
  • GB/T 14996 (2010) - Cold-Rolled heat-resisting superalloy sheets

Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH3128 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Cr 19.0 22.00
Mo 7.50 9.00
Ni - Remainder
W 7.50 9.00
Al 0.40 0.80
Ti 0.40 0.80
Fe - 2.0
Si - 0.80
Mn - 0.50
P - 0.013
S - 0.013
B - 0.005
Ce - 0.05
Zr - 0.06

GH3128 - Detail

GH3128

Mechanical properties of grade GH3128 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
614 (≥) 322 (≥) 23 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade GH3128 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
463 (≥) 193 (≥) 42 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
974 813 715

Equivalent Grade

Equivalent Products

We can customize the production of GH3128 grade, contact us for the best solution.