GH4118 Superalloys

GH4118 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH4118 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Cr 14.0 16.0
Mo 3.0 5.0
Ni - Remainder
Co 13.5 15.5
Al 4.5 5.0
Ti 3.5 4.5
B 0.01 0.025
Fe - 0.1
Zr - 0.15

GH4118 - Detail

GH4118

Mechanical properties of grade GH4118

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
573 (≥) 175 (≥) 34 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade GH4118

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
847 (≥) 515 (≥) 41 44 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
126 524 199

Equivalent Grade

Equivalent Products

We can customize the production of GH4118 grade, contact us for the best solution.
sales@specificsteel.com