HNVl Stainless Steels

HNVl - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of HNVl grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.55
Si 1.50
Mn 0.40
P
S
Cr 8.00
Mo 0.75

HNVl - Detail

Steel for intake valves

Mechanical properties of grade HNVl

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
683 (≥) 293 (≥) 32 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade HNVl

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
741 (≥) 524 (≥) 43 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
515 826 528

Equivalent Products

We can customize the production of HNVl grade, contact us for the best solution.