HR402 Stainless Steels to BS HR 402 (1973)

HR402 - Specification & Application

  • BS HR 402 (1973) - Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy cold worked and softened seamless tubes (nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)
  • BS 2HR 402 (2011) - Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Chemical composition(wt.%) of HR402 grade: to BS HR 402 (1973)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.13
Si - 1.00
Mn - 1.00
P - -
S - 0.015
Cr 18.00 21.00
Ni - remaining
Mo - -
Co 15.00 21.00
Ti 2.00 3.00
Fe - 1.50
Al 1.00 2.00
Cu - 0.20
Zr - 0.15
B - 0.02
Bi - 0.0001
Pb - 0.002
Ag - 0.0005

HR402 - Detail

Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Mechanical properties of grade HR402 BS HR 402 (1973)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
754 (≥) 359 (≥) 24 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade HR402 BS HR 402 (1973)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
226 (≥) 152 (≥) 22 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
775 474 739

Equivalent Grade

Equivalent Products

We can customize the production of HR402 grade, contact us for the best solution.
sales@specificsteel.com