HR404 Stainless Steels to BS HR 404 (1973)

HR404 - Specification & Application

  • BS HR 404 (1973) - Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy cold worked solution treated seamless tubes (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)
  • BS 2HR 404 (2011) - Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy cold worked solution treated seamless tubes (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy cold worked solution treated seamless tubes (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Chemical composition(wt.%) of HR404 grade: to BS HR 404 (1973)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.40
Mn - 0.60
P - -
S - 0.007
Cr 19.00 21.00
Ni - remaining
Mo 5.60 6.10
Co 19.00 21.00
Ti 1.90 2.40
Fe - 0.70
Al 0.30 0.60
Ag - 0.0005
Al+Ti 2.40 2.80
Cu - 0.20
B - 0.0050
Bi - 0.0001
Pb - 0.002

HR404 - Detail

Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy cold worked solution treated seamless tubes (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Mechanical properties of grade HR404 BS HR 404 (1973)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
824 (≥) 516 (≥) 21 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade HR404 BS HR 404 (1973)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
955 (≥) 371 (≥) 43 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
635 363 973

Equivalent Grade

Equivalent Products

We can customize the production of HR404 grade, contact us for the best solution.