Inconel 722 Superalloys to AMS 5411

Inconel 722 - Specification & Application

  • AMS 5411 - Nickel Inconel 722 AMS 5541 Strip

Used for gas turbine structural components, such as turbine section frames. The alloy is useful where oxidation resistance and high temperature strength are of major importance.

Chemical composition(wt.%) of Inconel 722 grade: to AMS 5411

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.07
Mn - 1.00
Cr 14.00 17.00
Ni - Balance
Cu - 0.5
Fe 5.00 9.00
P - -
S - 0.01
Ti 2 2.75
Al 0.40 1.00

Inconel 722 - Detail

Physical Data : [top]

 
 
Density (lb / cu. in.) 0.298
Specific Gravity 7.95
Specific Heat (Btu/lb/Deg F - [32-212 Deg F]) 0.105
Electrical Resistivity (microhm-cm (at 68 Deg F)) 750
Melting Point (Deg F) 2550
Thermal Conductivity 102
Mean Coeff Thermal Expansion 5.8
Magnetic Permeability 1.002
Modulus of Elasticity Tension 31

Mechanical properties of grade Inconel 722 AMS 5411

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
471 (≥) 782 (≥) 32 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade Inconel 722 AMS 5411

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
381 (≥) 197 (≥) 12 32 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
597 987 963

Equivalent Products

We can customize the production of Inconel 722 grade, contact us for the best solution.