LWCF21 Stainless Steels to BS 6323-8

LWCF21 - Specification & Application

  • BS 6323-8 - Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Chemical composition(wt.%) of LWCF21 grade: to BS 6323-8

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.50 19.00
Ni 8.00 11.00
Mo - -

LWCF21 - Detail

Specification for seamless and welded steel tubes for automobile , mechanical and general engineering purposes. Specific requirements for longitudinally welded stainless steel tubes

Mechanical properties of grade LWCF21 BS 6323-8

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
626 (≥) 514 (≥) 41 41 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade LWCF21 BS 6323-8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
757 (≥) 324 (≥) 14 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
912 748 138

Equivalent Products

We can customize the production of LWCF21 grade, contact us for the best solution.